Mike Miller wrote:
Abrigon Gusiq wrote in message ... Can you glassify Aluminium? Plain aluminum? Sure, in ultra-thin foils by splat cooling and other ultra-fast cooling techniques. Pure elemental metals and lightly alloyed materials crystallize very, very fast. You need cooling rates on the order of 1 million degrees per second to glassify them. Has any work been done on CVD of glassy metals? |